[DeTomaso] filling spot welds

Justin Greisberg justingreisberg at hotmail.com
Mon Feb 14 14:40:30 EST 2011


probably all good points.  if you look at a master metal worker, they do more with lead than fillers.  it is art, and i tried it on my spot welds with fair results.  probably mostly just makes me feel good about it.  i bet you can do fine with fillers here, especially something like fiberglass which might be less likely to crack.  but lead isnt all that hard to fill a hole, and I hope will never crack.  having done all my metal work and painting myself on my car, i would use lead again for filling bigger holes or gaps, and use the body filler just in a thin coat to make it look nice
 
 
 

 
> From: cmccann1972 at gmail.com
> To: rimov at charter.net; justingreisberg at hotmail.com; detomaso at realbig.com
> Subject: RE: [DeTomaso] filling spot welds
> Date: Mon, 14 Feb 2011 11:38:39 -0600
> 
> I have had some experience with various fillers, and I would like to back up
> what Paul R. says here...Duraglass is a great product. It's very important
> to note that not all "body fillers" are created equal. Some perform very
> well for skim coats, some perform fine in thicknesses up to an 1/8th inch,
> if you can tolerate knowing it's there. Some perform better at bare metal
> only and some are just fine over primers...some tolerate some flexing and
> have a higher plasticity and others are more brittle....just need to do
> research on the right product and application based off of the condition of
> your car and go from there. In general the Duraglass is a great place to
> start...but it needs a lot of "tooth" for proper adhesion. A lot of people
> judge all body fillers by the performance of incorrectly applied "Bondo".
> The spot welds are ABSOUTELY capable of being filled without risk of
> separation....if the right product is chosen and applied the right way...
> 
> My two cents...
> 
> Cullen
> Rust project 3925
> 
> 
> 
> 
> 
> 
> Subject: Re: [DeTomaso] filling spot welds
> 
> I would highly recommend using Duraglass. It is a fiberglass reinforced 
> resin filler. Easy to use, lightweight, durable and fills the dimples 
> extremely well. I did my engine bay many years ago with it and it was 
> excellent to work with. For best results it is best to top coat with a super
> 
> thin layer of plastic filler then high build primer.
> 
> Paul
> 
 		 	   		  